Production Technology Watch — week of November 2, 2026
Ten production and scale-up updates this week, including PFAS-free dry coating for sodium-ion electrodes, 100 mm AlN wafers, an all-electric glass plant and a large chlor-alkali start-up.
Ten production and scale-up updates this week, including PFAS-free dry coating for sodium-ion electrodes, 100 mm AlN wafers, an all-electric glass plant and a large chlor-alkali start-up.
A practical guide to the two binders in water-based graphite anodes: what the CMC grade and the SBR dose each control, what the flow curve shows, and how drying moves the binder.
A 300 mm GaN power fab, a 100 MWh solid-state cell line, lignin-based hard carbon and more production news from the week.
Why the same MOF binder dose works in one formulation and fails in the next: solids loading, binder–surface chemistry and pre-coated crystals, from three recent studies.
Ten production-technology developments: lab-to-line electrode coating windows, LFP cell commissioning in Morocco, US high-purity mineral refining, automated refractory pressing, ammonia reformer revamps, a MOF-desiccant field test and more.
Ten production-technology developments this week: solid-state cells on a converted Li-ion line, bio-based synthetic graphite, new 300 mm fabs, MLCC expansion, ethenolysis at scale, green-ammonia compression and more.
How to read a battery electrode slurry flow curve region by region for slot-die coating — what recent rheology research adds, a measurement checklist, and where the flow curve stops being enough.
Published optimum dispersant dosages vary several-fold between systems. A practical sequence for finding a working dosage for tape-casting and slip-casting slurries, and the side effects to check.
Pressing, granulation and extrusion all cost MOF surface area — how much depends on the framework and the binder. A process reading of published data and a recent extrusion patent.